Tubus linearis chalybis carbonis API 5L Gr. B/X42 /X52 /X60 /X65 Psl2
| Gradus | API 5L Gradus B, X42, X52, X56, X60, X65, X70, X80 |
| Gradus Specificationis | PSL1, PSL2 |
| Ambitus Diametri Externi | A dimidio uncia ad duas uncias, tres uncias, quattuor uncias, sex uncias, octo uncias, decem uncias, duodecim uncias, sedecim uncias, duodeviginti uncias, viginti uncias, viginti quattuor uncias usque ad quadraginta uncias. |
| Crassitudinis Ordo | SCH 10, SCH 20, SCH 40, SCH STD, SCH 80, SCH XS, ad SCH 160 |
| Genera Fabricationis | Sine sutura (calido laminata et frigido laminata), ERW sudatum (resistentia electrica sudatum), SAW (arcu submerso sudatum) in LSAW, DSAW, SSAW, HSAW |
| Typus Finis | Extrema obliqua, extrema plana |
| Ambitus Longitudinis | SRL (Longitudo Singularis Fortuita), DRL (Longitudo Duplex Fortuita), 20 pedes (6 metra), 40 pedes (12 metra) vel, ad singulorum necessitates aptata. |
| Pilei Protectionis | plastica vel ferrum |
| Curatio Superficiei | Naturalis, Vernis, Nigra Pictura, FBE, 3PE (3LPE), 3PP, CWC (Concrete Weight Coated) CRA Obductus vel Lineatus |
Tubus API 5L ad tubum chalybis carbonis, in systematibus transmissionis olei et gasi adhibitum, refertur. Adhibitur etiam ad transportanda alia fluida, ut vaporem, aquam et lutum.
Specificatio API 5L et genera fabricationis conglutinatarum et sine suturis amplectitur.
Genera Coniuncta: ERW, SAW, DSAW, LSAW, SSAW, HSAW Fistula
Typicae varietates tuborum API 5L conglutinatorum infra sunt:
REG (vel fortasse "ERW")Soldatura resistentiae electricae adhibetur in tubis cuius diametrum minus quam 24 unciarum.
DSAW/ SAWSoldatura arcus submersi utrinque/soldatura arcus submersi est alia methodus soldaturae quae loco ERW pro tubis magni diametri adhiberi potest.
LSAWSoldatura longitudinalis submersa per arcum electricum ad tubum usque ad 48 digitos in diametro adhibetur. Processus formationis JCOE appellatur.
SSAW/HSAWSoldatura arcus submersi spiralis/soldatura arcus submersi spiralis tubi usque ad 100 uncias in diametro.
Genera Tuborum Sinsutorum: Tubus Sinsutorum Calido-Laminatus et Tubus Sinsutorum Frigido-Laminatus
Tubus sine suturis typice adhibetur pro tubis parvi diametro (plerumque minus quam 24 unciae).
(Tubus ferreus sine suturis saepius quam tubus conglutinatus adhibetur pro diametris tuborum minoribus quam 150 mm (6 unciae).)
Tubos etiam sine suturis magni diametri offerimus. Processu fabricationis calido-laminato utentes, tubos sine suturis usque ad 20 uncias (508 mm) diametro producere possumus. Si tubos sine suturis maiores quam 20 uncias diametro requiris, eos processu calido-expanso usque ad 40 uncias (1016 mm) diametro producere possumus.
API 5L gradus sequentes specificat: Gradum B, X42, X46, X52, X56, X60, X65, X70, et X80.
Multae variae classes ferri pro tubis ferreis API 5L exstant, ut Gradus B, X42, X46, X52, X56, X60, X65, X70, et X80. Cum gradus ferri augeatur, moderatio aequivalentis carbonis strictior fit, et robur mechanicum maior.
Praeterea, compositio chemica tuborum API 5L sine suturis et conglutinatorum pro certo gradu non eadem est; tubus conglutinatus postulata altiora et minorem quantitatem carbonis et sulphuris habet.
Compositio Chemica pro tubo PSL 1 cum t ≤ 0.984” | |||||||
| Gradus Chalybis | Fractio massae, % secundum analysis caloris et producti a, g | ||||||
| C | Mn | P | S | V | Nb | Ti | |
| Maximus b | Maximus b | maximum | maximum | maximum | maximum | maximum | |
| Tubus sine sutura | |||||||
| A | 0.22 | 0.9 | 0.03 | 0.03 | – | – | – |
| B | 0.28 | 1.2 | 0.03 | 0.03 | c, d | c, d | d |
| X42 | 0.28 | 1.3 | 0.03 | 0.03 | d | d | d |
| X46 | 0.28 | 1.4 | 0.03 | 0.03 | d | d | d |
| X52 | 0.28 | 1.4 | 0.03 | 0.03 | d | d | d |
| X56 | 0.28 | 1.4 | 0.03 | 0.03 | d | d | d |
| X60 | 0.28 e | 1.40 e | 0.03 | 0.03 | f | f | f |
| X65 | 0.28 e | 1.40 e | 0.03 | 0.03 | f | f | f |
| X70 | 0.28 e | 1.40 e | 0.03 | 0.03 | f | f | f |
| Tubus Soldatus | |||||||
| A | 0.22 | 0.9 | 0.03 | 0.03 | – | – | – |
| B | 0.26 | 1.2 | 0.03 | 0.03 | c, d | c, d | d |
| X42 | 0.26 | 1.3 | 0.03 | 0.03 | d | d | d |
| X46 | 0.26 | 1.4 | 0.03 | 0.03 | d | d | d |
| X52 | 0.26 | 1.4 | 0.03 | 0.03 | d | d | d |
| X56 | 0.26 | 1.4 | 0.03 | 0.03 | d | d | d |
| X60 | 0.26 e | 1.40 e | 0.03 | 0.03 | f | f | f |
| X65 | 0.26 e | 1.45 e | 0.03 | 0.03 | f | f | f |
| X70 | 0.26e | 1.65 e | 0.03 | 0.03 | f | f | f |
| a. Cu ≤ = 0.50% Ni; ≤ 0.50%; Cr ≤ 0.50%; et Mo ≤ 0,15%; | |||||||
| b. Pro qualibet reductione 0.01% infra concentrationem maximam specificatam pro carbone, augmentum 0.05% supra concentrationem maximam specificatam pro Mn permittitur, usque ad maximum 1.65% pro gradibus ≥ L245 vel B, sed ≤ L360 vel X52; usque ad maximum 1.75% pro gradibus > L360 vel X52, sed < L485 vel X70; et usque ad maximum 2.00% pro gradu L485 vel X70. | |||||||
| c. Nisi aliter convenerit, NB + V ≤ 0.06%, | |||||||
| d. Nb + V + TI ≤ 0.15%, | |||||||
| e. Nisi aliter convenerit. | |||||||
| f. Nisi aliter convenerit, NB + V = Ti ≤ 0.15%, | |||||||
| g. Nulla additio deliberata B permittitur et B residuum ≤ 0.001%. | |||||||
| Compositio Chemica pro tubo PSL 2 cum t ≤ 0.984” | |||||||||||||||||||||
| Gradus Chalybis | Fractio massae, % secundum analysis caloris et producti | Aequivalens Carbonis | |||||||||||||||||||
| C | Si | Mn | P | S | V | Nb | Ti | Alia | CE IIW | CE PCM | |||||||||||
| Maximus b | maximum | Maximus b | maximum | maximum | maximum | maximum | maximum | maximum | maximum | ||||||||||||
| Tubus sine suturis et conglutinatus | |||||||||||||||||||||
| BR | 0.24 | 0.4 | 1.2 | 0.025 | 0.015 | c | c | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| X42R | 0.24 | 0.4 | 1.2 | 0.025 | 0.015 | 0.06 | 0.05 | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| BN | 0.24 | 0.4 | 1.2 | 0.025 | 0.015 | c | c | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| X42N | 0.24 | 0.4 | 1.2 | 0.025 | 0.015 | 0.06 | 0.05 | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| X46N | 0.24 | 0.4 | 1.4 | 0.025 | 0.015 | 0.07 | 0.05 | 0.04 | d,e,l | 0.43 | 0.25 | ||||||||||
| X52N | 0.24 | 0.45 | 1.4 | 0.025 | 0.015 | 0.1 | 0.05 | 0.04 | d,e,l | 0.43 | 0.25 | ||||||||||
| X56N | 0.24 | 0.45 | 1.4 | 0.025 | 0.015 | 0.10f | 0.05 | 0.04 | d,e,l | 0.43 | 0.25 | ||||||||||
| X60N | 0.24f | 0.45f | 1.40f | 0.025 | 0.015 | 0.10f | 0.05f | 0.04f | g, h, l | Ut convenerat | |||||||||||
| BQ | 0.18 | 0.45 | 1.4 | 0.025 | 0.015 | 0.05 | 0.05 | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| X42Q | 0.18 | 0.45 | 1.4 | 0.025 | 0.015 | 0.05 | 0.05 | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| X46Q | 0.18 | 0.45 | 1.4 | 0.025 | 0.015 | 0.05 | 0.05 | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| X52Q | 0.18 | 0.45 | 1.5 | 0.025 | 0.015 | 0.05 | 0.05 | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| X56Q | 0.18 | 0.45f | 1.5 | 0.025 | 0.015 | 0.07 | 0.05 | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| X60Q | 0.18f | 0.45f | 1.70f | 0.025 | 0.015 | g | g | g | h,l | 0.43 | 0.25 | ||||||||||
| X65Q | 0.18f | 0.45f | 1.70f | 0.025 | 0.015 | g | g | g | h,l | 0.43 | 0.25 | ||||||||||
| X70Q | 0.18f | 0.45f | 1.80f | 0.025 | 0.015 | g | g | g | h,l | 0.43 | 0.25 | ||||||||||
| X80Q | 0.18f | 0.45f | 1.90f | 0.025 | 0.015 | g | g | g | i,j | Ut convenerat | |||||||||||
| X90Q | 0.16f | 0.45f | 1.9 | 0.02 | 0.01 | g | g | g | j,k | Ut convenerat | |||||||||||
| X100Q | 0.16f | 0.45f | 1.9 | 0.02 | 0.01 | g | g | g | j,k | Ut convenerat | |||||||||||
| Tubus Soldatus | |||||||||||||||||||||
| BM | 0.22 | 0.45 | 1.2 | 0.025 | 0.015 | 0.05 | 0.05 | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| X42M | 0.22 | 0.45 | 1.3 | 0.025 | 0.015 | 0.05 | 0.05 | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| X46M | 0.22 | 0.45 | 1.3 | 0.025 | 0.015 | 0.05 | 0.05 | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| X52M | 0.22 | 0.45 | 1.4 | 0.025 | 0.015 | d | d | d | e,l | 0.43 | 0.25 | ||||||||||
| X56M | 0.22 | 0.45f | 1.4 | 0.025 | 0.015 | d | d | d | e,l | 0.43 | 0.25 | ||||||||||
| X60M | 0.12f | 0.45f | 1.60f | 0.025 | 0.015 | g | g | g | h,l | 0.43 | 0.25 | ||||||||||
| X65M | 0.12f | 0.45f | 1.60f | 0.025 | 0.015 | g | g | g | h,l | 0.43 | 0.25 | ||||||||||
| X70M | 0.12f | 0.45f | 1.70f | 0.025 | 0.015 | g | g | g | h,l | 0.43 | 0.25 | ||||||||||
| X80M | 0.12f | 0.45f | 1.85f | 0.025 | 0.015 | g | g | g | i,j | .043f | 0.25 | ||||||||||
| X90M | 0.1 | 0.55f | 2.10f | 0.02 | 0.01 | g | g | g | i,j | – | 0.25 | ||||||||||
| X100M | 0.1 | 0.55f | 2.10f | 0.02 | 0.01 | g | g | g | i,j | – | 0.25 | ||||||||||
| a. SMLS t > 0.787", limites CE erunt ut conventa sunt. Limites CEIIW adhibentur si C > 0.12% et limites CEPcm valent si C ≤ 0.12%, | |||||||||||||||||||||
| b. Pro qualibet reductione 0.01% infra maximum definitum pro C, augmentum 0.05% supra maximum definitum pro Mn permittitur, usque ad maximum 1.65% pro gradibus ≥ L245 vel B, sed ≤ L360 vel X52; usque ad maximum 1.75% pro gradibus > L360 vel X52, sed < L485 vel X70; usque ad maximum 2.00% pro gradibus ≥ L485 vel X70, sed ≤ L555 vel X80; et usque ad maximum 2.20% pro gradibus > L555 vel X80. | |||||||||||||||||||||
| c. Nisi aliter convenerit, Nb = V ≤ 0.06%, | |||||||||||||||||||||
| d. Nb = V = Ti ≤ 0.15%, | |||||||||||||||||||||
| e. Nisi aliter convenerit, Cu ≤ 0.50%; Ni ≤ 0.30% Cr ≤ 0.30% et Mo ≤ 0.15% | |||||||||||||||||||||
| f. Nisi aliter convenit, | |||||||||||||||||||||
| g. Nisi aliter convenerit, Nb + V + Ti ≤ 0.15%, | |||||||||||||||||||||
| h. Nisi aliter convenerit, Cu ≤ 0.50% Ni ≤ 0.50% Cr ≤ 0.50% et MO ≤ 0.50% | |||||||||||||||||||||
| i. Nisi aliter convenerit, Cu ≤ 0.50% Ni ≤ 1.00% Cr ≤ 0.50% et MO ≤ 0.50% | |||||||||||||||||||||
| j. B ≤ 0.004%, | |||||||||||||||||||||
| k. Nisi aliter convenerit, Cu ≤ 0.50% Ni ≤ 1.00% Cr ≤ 0.55% et MO ≤ 0.80% | |||||||||||||||||||||
| 1. Omnibus gradibus tuborum PSL 2, exceptis illis gradibus in adnotationibus j notatis, sequentia valent. Nisi aliter convenerit, nulla additio intentionalis B permittitur et B residuum ≤ 0.001%. | |||||||||||||||||||||
| PSL | Status Partus | Gradus tubi |
| PSL1 | Sicut volutatum, normalizatum, normalizans formatum | A |
| Secundum laminationem, laminatione normalizanti volutata, laminatione thermomechanica volutata, formatione thermomechanica formata, formatione normalizanti formata, normalizata, normalizata et temperata, vel si convenerit, secundum qualitatem et modum tractationem (SMLS) tantum. | B | |
| Secundum laminationem, normalizando volutatum, thermomechanice volutatum, thermomechanice formatum, normalizando formatum, normalizatum, normalizatum et temperatum | X42, X46, X52, X56, X60, X65, X70 | |
| PSL 2 | Ut volutatum | BR, X42R |
| Normalizatio volubilis, normalizatio formata, normalizata vel normalizata et temperata | BN, X42N, X46N, X52N, X56N, X60N | |
| Extinctum et temperatum | BQ, X42Q, X46Q, X56Q, X60Q, X65Q, X70Q, X80Q, X90Q, X100Q | |
| Thermomechanice volutata vel thermomechanice formata | BM, X42M, X46M, X56M, X60M, X65M, X70M, X80M | |
| Thermomechanica volutata | X90M, X100M, X120M | |
| Sufficit (R, N, Q vel M) pro gradibus PSL2 ad gradum chalybis pertinet. |
PSL1 et PSL2 differunt tam in ambitu probationis quam in proprietatibus chemicis et mechanicis.
PSL2 strictior est quam PSL1 in compositione chemica, proprietatibus tensilibus, probatione impactus, probatione non destructiva et cetera.
Examen Impactus
Solum PSL2 probationem impactus requirit: praeter X80.
NDT: Examinatio Non Destructiva. PSL1 examinationem non destructivam non requirit si examinationem non destructivam applicabilem esse non requirit. PSL2 autem applicat.
(Examinatio non destructiva: Examinatio non destructiva et examinatio secundum normam API 5L utitur methodis radiographicis, ultrasonicis, vel aliis (sine materia destruenda) ad defectus et imperfectiones in canalibus detegendas.)
Involucrum estplerumque nudus, vinculum filum ferreum, valdefortis.
Si requisita specialia habes, uti potesinvolucrum rubiginis impervium... et pulchriores.
Cautelae in involucris et transportatione tuborum chalybis carbonis
1.Tubus Ferreus API 5LA damno a collisione, extrusione et incisionibus durante transportatione, conservatione et usu effectis protegendum est.
2. Dum tubos chalybis carbonis tractas, explosionibus, incendiis, veneficiis, aliisque accidentibus attendere debes, et praecepta operationis securitatis sequi.
3. Dum utitur,Tubus chalybis carbonis API 5LContactum cum temperaturis altis, mediis corrosivis, et cetera vitare debet. Si in his ambitus adhibeantur, tubi chalybis carbonis ex materiis specialibus facti, ut resistentia temperaturae altae et resistentia corrosionis, eligendi sunt.
4. Tubus chalybis carbonis electus materiae et specificationis idoneae fieri debet secundum factores comprehensivos, inter quos ambitus usus, natura medii, pressio, temperatura, et cetera.
5. Antequam tubus chalybis carbonis adhibeatur, inspectiones et probationes necessariae peragendae sunt ut qualitas eius secundum normam sit comprobetur.
Vectura:Celer (Traditio Exemplaris), Aerea, Ferrea, Terrestre, Maritima (FCL vel LCL vel Massa)
Q: Suntne fabricatores UA?
A: Ita, fabricatores tuborum ferreorum spiralium sumus, in vico Daqiuzhuang, urbe Tianjin, Sinis siti.
Q: Possumne mihi mandatum experimentale tantum aliquot tonnas habere?
A: Scilicet. Onus tibi per ministerium LCL mittere possumus. (Minus onus continentis)
Q: Si exemplum gratuitum?
A: Exemplar gratuitum, sed emptor pro vectura solvit.
Q: Esne auri praebitor et mercaturam fideiussorem facis?
A: Tredecim annos auri praebitores sumus et commercium fideiussorem accipimus.